Separation Efficiency
Quantitative measurement of an adhesive layer’s ability to release cleanly from a container substrate during alkaline washing defines its recycling compatibility. This de-linking performance establishes whether pressure-sensitive labels, heat-seal lacquers, or functional barriers detach from polymer and fibre substrates without leaving tackified residues. The assessment evaluates adhesive fragmentation, release speed, and residue levels remaining on recovered flakes or pulp fibres.
Test conditions follow standardized washing protocols, typically at 65 to 85 degrees Celsius in a 1 to 2 percent sodium hydroxide bath under mechanical agitation. Complete release ensures recovered materials maintain purity limits set for closed-loop food-grade packaging resins.
Interfacial Debonding
Caustic wash solution penetrates the boundary between adhesive and packaging walls. De-linking performance relies on temperature-activated swelling or chemical breakdown within the adhesive polymer matrix. As the alkaline solution infiltrates the interface, hydrophilic domains in the formulation absorb liquid and generate localized shear stresses that overcome van der Waals bonding.
Cross-linked wash-off adhesives peel away in intact films rather than dissolving into fine tackified particles. Uncrosslinked formulations risk gumming screens and adhering to clean polymer flakes during separation stages. High de-linking values prevent adhesive redeposition onto PET or polyolefin flakes during flotation and rinsing stages.
Substrate Recovery
Verification of clean release protects automated sorting systems and final pellet clarity. In automated flake sorting lines, residual adhesive causes optical discolouration, thermal degradation, and black specks during melt extrusion. High de-linking metrics correlate directly with reduced haze in thermoformed rPET sheet production and lower volatile organic compound emissions during pellet devolatilization.
Adhesives that resist caustic detachment leave residues that foul wash tanks, clog dewatering sieves, and compromise secondary bonding in recycled packaging structures.