Surface Imperfection
Small circular depressions in the coating layer of a paper substrate constitute pinoid pits. These indentations occur when air bubbles or organic contaminants disrupt the uniform flow of the slurry across the paper surface during the manufacturing process. Such irregularities compromise the surface smoothness of the finished stock and result in visible voids within the printed image.
Production Cause
Mechanical agitation in the supply line introduces microscopic pockets of trapped gas into the pigment coating. Coating formulations with high viscosity fail to redistribute the material effectively once these bubbles burst against the base sheet. Drying temperatures that rise too quickly trap residual gases within the film before the binder achieves proper crosslinking.
Heavy weight sheets often exhibit higher instances of this defect due to the thicker application layers required for high-speed printing.
Performance Impact
Printers encounter significant difficulties when applying high-tack inks to substrates containing these cratered zones. The lack of material in the pits leads to skips in the halftone screen and inconsistent dot gain across the sheet. Large solid areas of color highlight the contrast between the coated surface and the exposed paper base beneath the void.
Precise control of the blade pressure and flow rate reduces the occurrence of these pits in high-quality print stocks.