Fibrillation Junction
Physical positions across multi-disc or conical refiner systems designated as refining nodes deliver mechanical energy directly to cellulose fibre slurries within stock preparation plants. A refining node encompasses the operational shear volume formed between rotating rotor bars and fixed stator plates through which pulp suspensions pass under controlled hydraulic pressure. These mechanical processing zones exert compression, shear, and peeling stresses that develop fibre flexure and delaminate internal cell walls.
The mechanical scope is limited to the active bar crossing zone, excluding unpressurized feed housings and external slurry distribution piping.
Mechanical Action
Cellulosic fibres enter the narrowing gap between rotor and stator bars where bar edges trap fibre flocs under intense hydrodynamic shear. Specific edge load and net specific energy input define the mechanical intensity inside the refining node. High specific edge loads shear primary cell walls, producing external fibrillation and shortening long softwood tracheids, while lower edge loads promote internal swelling without cutting.
Centrifugal force pushes the slurry outward across bar surfaces, while crossing angles generate pressure pulses that expel water from fiber wall layers. Operators vary disc gaps down to micron increments to govern mechanical impact intensity without causing bar-to-bar contact.
Stock Preparation
Adjusting the number of active nodes in series controls sheet density, porosity, and tensile strength development across bleached kraft pulp runs. Packaging mills processing recycled linerboard modulate node gaps to hydrate old corrugated container fibres, recovering bonding capacity lost during prior drying cycles. In contrast, under-refining at these nodes leaves fibres stiff, producing bulky sheets with low Mullen burst values that split under score-line creasing on carton gluers.
Excessive processing within nodes generates broken fine material that blinds forming fabrics and degrades dewatering rates. Precise bar pattern selection across refining nodes balances optical opacity against burst resistance across industrial packaging grades.