Boundary Discontinuity
Interfacial velocity differentials develop when fluid layers adjacent to solid boundary walls move at different speeds from the physical surfaces enclosing them. Rotational viscometry and capillary extrusion of high-solids paperboard coatings experience wall slip due to steric depletion of pigment particles away from smooth instrument walls. A low-viscosity liquid boundary layer forms against the metal surface, lubricating the bulk fluid and causing the suspension to slide as a plug.
The phenomenon invalidates standard fluid calculations that assume zero relative velocity between fluids and solid boundaries, ceasing to apply only when fluid boundary adherence matches bulk velocity fields.
Depletion Layer
Large pigment particles, kaolin clays, and calcium carbonates cannot pack their geometric centers directly against a solid metal wall. This steric hindrance creates a narrow, particle-depleted zone against the wall composed predominantly of water and soluble binders. The depleted boundary layer possesses a lower dynamic viscosity than the concentrated bulk slurry filling the remainder of the measuring gap.
Under applied shear stress, deformation concentrates inside this thin lubrication layer, allowing the concentrated core to translate with minimal internal shear. Rotational rheometers record artificially depressed torque values, underestimating true suspension viscosity across broad shear regimes. Verifying slip involves testing samples in identical geometries with varied gap dimensions or comparing smooth surfaces against grooved or serrated boundary geometries that pin the bulk suspension.
Coating Defects
Accurate measurement of paper coating rheology requires eliminating wall slip to prevent misjudging the formulation performance on industrial application stations. Slurry that slips along delivery pipes and metering blades creates uneven hydrodynamic lift, generating irregular coat weight distribution, blade chatter, and coating streaks across the paperboard web. Converting laboratories use serrated bob-and-cup geometries to anchor mineral slurries, ensuring that measured shear reflects true bulk fluid deformation.
In extrusion coating of barrier polymers onto packaging board, wall slip induces sharkskin defects and melt fracture that compromise moisture and grease resistance. Formulators introduce chemical processing aids and adjusting solids distributions to mitigate slip tendencies along metal machinery walls. Managing wall slip ensures that laboratory rheometer tests predict commercial runnability of high-solids coatings across paperboard converting machinery.