Creasing Channel
Tooling specifications in creasing equipment designate the pre-formed channel that receives paperboard fibers pushed by a male creasing rule. In carton converting operations, female matrix groove dimensions dictate the depth and width of fold lines formed across solid bleached board or recycled paperboard grades. Proper groove geometry allows paperboard plies to shear internally without rupturing the outer linerboard.
When channel width proves too narrow, high score stiffness causes liner cracking along the creasing axis.
Board Clearance
Converting accuracy depends on matching channel dimensions to substrate thickness and grain direction. Packaging engineers select female matrix groove widths based on twice the board caliper plus rule thickness for cross-grain creases, adjusting for liner stiffness. Deep grooves allow full penetration of male creasing rules, inducing controlled internal delamination across paperboard plies.
Substrates with high starch content require wider channels to prevent surface tearing during folding operations. Precise positioning of matrix strips onto cutting plates eliminates score misplacement, reducing waste on high-speed platen presses.
Delamination Mechanism
Internal ply separation during score formation determines how easily cartons fold on automatic packaging lines. Channel depth within female matrix groove tooling governs the volume of board displaced during the creasing stroke. Insufficient channel clearance causes outer liner rupture during folding.