Gravimetric Desiccation Method
Standardized determination of the volatile matter mass fraction in paper, board, and pulp specimens relies on oven-drying at regulated thermal conditions until the sample reaches constant weight. Specified by international consensus, iso 638 moisture content measurement dictates exposure of prepared test pieces to a circulating air temperature of one hundred and five degrees Celsius. The test measures the percentage of water mass lost relative to the original sample weight before thermal exposure.
Finished corrugated board, virgin pulp bales, and solid bleached folding cartons must be evaluated using this exact procedure to avoid commercial disputes over billed moisture versus dry fibre weight. The scope governs standard paper and board products, excluding sheets treated with volatile compounds that evaporate under the same drying temperature.
Thermal Equilibration Mechanics
Laboratory technicians place weighing vessels inside desiccators to prevent atmospheric moisture absorption during the cool-down period preceding mass measurement. Constant mass is achieved when two consecutive weighings, separated by a specified heating interval, do not differ by more than zero point one percent of the initial specimen mass. Pulp bales delivered at nominal eighty-eight percent air-dry purity rely on this standard method to determine invoiced commercial weight corrections.
Packaging board samples are sealed in airtight moisture bags immediately upon cutting from reels to capture true machine-exit moisture states before ambient humidity shifts the reading.
Converting Stability Requirements
Sheet flatness, dimensional stability, and flexural stiffness directly correlate with the residual moisture left in paperboard reels. In corrugated converting plants, flute bonding and warp formation behave erratically if incoming linerboard departs from the five to eight percent moisture envelope defined by quality agreements. Excess moisture reduces the box compression test value of corrugated containers, whereas excessively dry liners crack along the scorelines during folder-gluer operations.
Iso 638 moisture content verification provides the absolute legal baseline for settlement whenever reel moisture variations trigger converting plant jams or delamination claims.