Extrusion Shear
Fluid motion of molten thermoplastic during extrusion coating forces air out of substrate pores to bond polymer film to paper board. Hydrodynamic polymer displacement occurs as molten resin exits a flat die and hits the moving paper web under high nip pressure. Applied compressive force drives liquid polymer into surface voids between cellulose fibers before thermal cooling solidifies the plastic layer.
Melt temperature and web speed dictate penetration depth across the substrate interface.
Interface Adhesion
Mechanical interlocking between paperboard and extruded film relies on polymer flow into porous paper structures. Controlling polymer displacement prevents excessive resin penetration into paperboard substrates while achieving robust adhesion strength. High extrusion temperatures reduce polymer melt viscosity, enabling rapid wetting of paper fibers within the narrow nip contact zone.
Chill roll cooling stops resin movement quickly, locking the polymer anchor points into fiber pores. Insufficient displacement yields poor bond strength, causing film peeling during packaging converting operations. Excessive resin penetration wastes raw material and reduces barrier coating thickness, compromising moisture and gas protection.
Converting line operators monitor resin melt temperature and nip compression to maintain target adhesion levels without damaging delicate paperboard surfaces.
Coat Weight
Resin volume applied per unit surface area dictates final barrier layer performance. Uniform melt distribution prevents gauge variation and pinhole formation across wide paperboard webs. Precise metering adjustments ensure target coat weight compliance across continuous coating runs.