Interlaminar Resistance
Mechanical energy required to separate internal plies of paperboard per unit area defines the fundamental resistance of multi-ply paper substrates against internal rupture during high-speed converting. Quantitative evaluation of delamination fracture energy isolates the z-directional bond strength governed by internal starch addition and fibre interlock across the thickness profile. Standardized laboratory testing applies controlled tensile or shear displacement to a pre-cracked specimen to monitor force against crack growth distance.
The measurement ceases to apply once failure transitions from internal ply division to surface fibre peeling or total web shear.
Separation Energy
Internal fibre orientation and localized density distribution determine how crack propagation travels between web layers. When mechanical stress concentration exceeds the internal bonding limit, micro-cracks form within the amorphous matrix of hydrogen bonds binding adjacent fibre networks. Higher delamination fracture energy prevents unexpected internal splitting when folding carton plies undergo sharp mechanical bending.
Softwood kraft fibres increase this threshold by contributing longer interlocking paths across the sheet interface.
Scoring Compliance
Board structures exhibiting insufficient energy resistance fail along crease lines during automated package assembly. Low delamination fracture energy causes wide ply separation along score channels, which creates unsightly bulges and weakens edge compression strength. Controlled internal cleavage allows clean folding without fracturing the outer linerboard layer during high-speed cartoning.