Polyisocyanate Crosslinker Density Adjustments for High Humidity Crease Crack Prevention in Coated Board
Balancing polyisocyanate addition at 3.5 to 4.5 percent solids maintains high-humidity barrier holdout while preserving the elongation needed to prevent score cracking.