Fibre Adhesion
Resistance to perpendicular tensile forces defines internal bond strength across paper and multi-ply packaging board structures. Z-directional tensile testing measures this property by pulling composite layers apart until perpendicular failure occurs within the substrate. Low values indicate poor interfiber bonding or inadequate refining during stock preparation, which leads to catastrophic delamination during high-speed printing or heavy adhesive application.
Plies Laminate
Multi-ply paperboard relies heavily on proper couch roll pressing and wet-end chemical retention to secure distinct sheet layers together during formation. When refiners apply excessive mechanical action to chemical pulp, individual fibers fracture rather than fibrillate, reducing the available surface area for hydrogen bonding across the central plane. Converters evaluate this internal cohesion to predict whether carton blanks will survive aggressive creasing operations without splitting along the edges under high converting speeds.
Resin Addition
Polyamine-epichlorohydrin wet-strength resins improve internal bond performance by creating covalent cross-links between cellulose fibers in aqueous environments. Papermakers adjust additive dosage rates based on furnish composition, because short recycled fibers require higher chemical reinforcement than virgin long-fiber furnishes to achieve equivalent delamination resistance. Finished packaging materials must maintain sufficient Z-directional strength to withstand torsional loads imposed by automated vacuum suction feeders on high-speed cartoning lines.