Predicting High-Speed Converting Delamination Failures from Dynamic Shear Energy and Steady Out-Of-Plane Tensile Discrepancies
Static Z-tensile tests fail at converting speeds because Mode II dynamic shear energy dissipation governs ply bond stability under microsecond strain rates.