Barrier Chemistry
Aqueous polymer formulations containing sub-micron particles of polyethylene or polypropylene suspended in water provide sealable surface barriers without requiring plastic film lamination. Applied using standard coating heads, polyolefin dispersions form continuous thin coatings on paper and folding carton stocks upon thermal drying and film coalescence. The dispersion eliminates the need for hot extrusion coating dies, letting printers coat water, grease, and heat-seal barriers inline on flexographic presses.
Coalesced dispersion coatings preserve substrate repulpability because the thin polymer layers break apart rapidly under the mechanical shear of conventional hydropulpers. The coating formulation behaves as an aqueous liquid during application, functioning as a solid barrier only after full water evaporation.
Film Formation Dynamics
Application via blade, rod, or air-knife coaters deposits the liquid suspension uniformly across the fibrous surface, where capillary action pulls water into the porous paper network. Evaporation inside convection drying tunnels forces suspended polyolefin spheres into close contact until capillary pressure deforms their spherical shells. Further heating above the polymer melting temperature fuses the softened particles into a pinhole-free barrier layer that bonds directly with surface fibres.
Surfactants and volatile neutralizing agents like dimethylethanolamine volatilize during drying, enhancing the final coating resistance to moisture. Controlling drying rates prevents mud-cracking, which occurs if water leaves the coating layer before polymer chains can interdiffuse.
Converting Performance
Treated carton stocks exhibit water vapour transmission rates low enough to protect dry foods, paired with Cobb values beneath five grams per square metre over sixty seconds. Sealing jaws activate the polymer layer at lower temperatures than conventional extruded polyethylene films, accelerating operations on form-fill-seal lines. Finished paperboard retains full repulpability under CEPI recycling protocols, yielding clean fibre recovery rates above ninety percent.
This dual performance balances functional moisture resistance with standard mill recyclability.