Delamination Fracture
Interlaminar separation within outer surface layers occurs when internal cohesive strength falls below applied shear stress during web converting or printing. Under mechanical shear loads parallel to the sheet face, skin shear failure separates paperboard surface plies or paper coating interfaces from the underlying fibrous base. Gravure nip pressures, high-tack lithographic offset blankets, and sharp folding operations generate shear forces that trigger this fracture.
The boundary of this mechanism is confined to the boundary between the top ply and adjacent structural plies, terminating where through-thickness tensile rupture takes over.
Mechanical Stress
Multi-ply forming configurations bond diverse furnish layers across wet pressing nips. When top layers contain highly refined bleached chemical pulp and interior layers hold unrefined mechanical pulp or secondary fibre, physical shear resistance depends upon fibre entanglement across the ply interface. High-speed printing nips generate tangential forces as viscous inks exit printing blankets, exerting localized peeling and planar shear.
Insufficient ply bonding allows the top surface skin to detach cleanly, wrapping around print cylinders or blistering carton creases during packaging assembly.
Laboratory Testing
Scott bond instruments and dynamic peel testers quantify shear resistance by measuring the mechanical energy absorbed during rapid surface layer cleavage. Low values point to excessive filler loading in sub-surface plies, improper starch spray application between wires, or uneven pressing profiles across couch rolls. Increasing the refining level on top-ply furnish improves inter-fibre crosslinking, elevating shear resistance.
Controlling moisture profiles prevents brittle interfaces from delaminating during high-speed web handling across converting lines.