Coating Operation
Metering and applying a one hundred percent active liquid adhesive across a moving substrate web joins materials without requiring a thermal drying tunnel. The web travels through an application unit comprising heated transfer rollers that shear the viscous solvent-free formulation into a continuous, thin liquid film. Conducting a solventless adhesive pass eliminates the solvent evaporation phase, allowing the freshly coated web to move immediately into a combining nip against a secondary paper, film, or foil layer.
The process requires chemical crosslinking between polyols and polyisocyanates, or ambient moisture capture, to complete adhesive solidifying. Application ceases when processing substrates cannot withstand nip pressure or when dealing with porous open papers that absorb liquid adhesives before crosslinking completes.
Metering Precision
Maintaining coating uniformity demands high mechanical precision across the application roll assembly. A smooth metering roll transfers a controlled liquid layer onto an oscillating sleeve, which passes the adhesive to a rubber applicator roll running at matching web speed. Application temperature regulates resin viscosity, requiring heating between forty and eighty degrees Celsius across internal water-circulated rolls.
Coating weights range between one and two grams per square meter, because excessive application results in adhesive squeeze-out and optical defects, while light application yields voids and poor bond integrity.
Operational Efficiency
Energy consumption decreases because operating without drying ovens eliminates high-volume heated air blowers and solvent recovery equipment. Converting facilities reduce volatile organic compound emissions, minimizing environmental compliance monitoring. Web tension control remains paramount when processing light paper grades combined with plastic films, as differing elastic properties can induce post-nip curling.
Controlled winding tension ensures laminated rolls cure without telescoping, air entrapment, or adhesive displacement across high-speed rewind stations.