Mathematical Relation
A mathematical calculation defines the optimal gap of a creasing matrix to prevent board splitting during folding operations. The channel width formula calculates this gap by multiplying the board thickness by a set factor and adding the width of the creasing rule. This standard formula helps carton manufacturers select the correct tooling for different grades of paperboard.
The formula remains valid only for standard solid bleached sulphate and duplex boards.
Mechanical Influence
Creasing rules press the board into the matrix channel to create a stable hinge. Applying the channel width formula incorrectly results in either a loose crease or ruptured linerboard. When the channel is too narrow, the board suffers high shear stress and cracks along the fold line.
Wide channels fail to squeeze the board enough, which causes poor fold registration on high speed packaging lines. This mechanical balance prevents delamination and ensures that the finished carton maintains its structural integrity on the filling machine.
Production Impact
Converters run these calculations before setting up the die-cutting press. The standard equation is width equals one point seven times board thickness plus rule thickness. Using this value ensures that the paperboard flows smoothly into the groove without tearing.
The resulting fold is clean and supports rapid gluing.