Refining Effect
Mechanical degradation of papermaking fibers through transverse shearing action in stock preparation equipment reduces average fiber length while altering suspension viscosity. Mill operators monitor fibre shortening during high-intensity refining where bar edge contacts cut cellulose walls rather than promoting internal fibrillation. Controlled cutting action increases sheet density and improves sheet formation at the expense of tearing strength.
Excessively cut fibers drain slowly on the Fourdrinier wire, creating web handling difficulties in the wet press section.
Morphological Change
Physical cutting occurs when fiber suspensions pass through narrow bar gaps under elevated specific edge loads inside disc or conical refiners. As mechanical energy transfers to the slurried stock, long softwood tracheids fragment into shorter segments, shifting the population distribution curve toward smaller length fractions. The resulting shift increases the total number of fiber ends per unit mass, which alters hydrogen bonding potential within the consolidating sheet network.
Shorter fibers fill interfiber voids, creating a tighter pore structure that enhances printability and opacity. However, shortened fibers exhibit decreased stress distribution capability across fractured paper regions during tensile failure testing.
Strength Limit
Tear resistance decreases linearly as the weighted average fiber length falls below critical thresholds established for specific paperboard grades. Excessive fibre shortening undermines the structural integrity of corrugated fluting and linerboard under dynamic converting loads.