Perpendicular Resistance
Compressive force applied perpendicular to the plane of single-wall corrugated board measures flute rigidity under standard laboratory conditions defined by ISO 3035 and TAPPI T 825. Conducting a flat crush test establishes the maximum resistance that fluted arches present against uniform crushing loads before complete structural collapse occurs. The procedure tests combined board rather than isolated papers or finished shipping boxes.
Test results do not correlate with box stacking performance because the loading axis runs parallel to the flute direction in warehouse storage.
Deformation Phases
Initial loading compresses surface liner irregularities before the flute arches enter a linear elastic deflection phase. The flat crush test records the peak force recorded when flute structures buckle, which is immediately followed by a steep drop in machine resistance as the medium flattens completely. Double-wall and triple-wall corrugated boards are excluded from this protocol because sequential collapse of unequal flute profiles yields multi-peak load curves that distort standard calculation models.
A low test value points to degraded corrugating medium stiffness, excessive pressure roll interference at the single facer, or moisture re-absorption along the converting line. Evaluating crush resistance across converted packaging identifies whether rotary die cylinders or printing impression rolls crushed the flutes during downstream fabrication. High medium formation uniformity produces steep initial load curves, whereas uneven fibre distribution causes premature localized buckling.
Laboratories condition circular test specimens at 23 degrees Celsius and 50 percent relative humidity to eliminate moisture-induced plasticization of cellulose fibres.
Structural Boundary
Specimen evaluation stops when flute walls fold into a horizontal plane and the platens compress the solid fibre mass. The flat crush test applies solely to structural fluting profiles and ceases to provide valid data if the circular test disc exhibits lateral shear failure or irregular perimeter crushing during the stroke.