Bending Stiffness
Displacement metrics describe outer ply movement relative to central neutral axes when multi-ply paperboard undergoes flexure. Excessive layer deflection indicates insufficient shear resistance between bleached chemical pulp liners and mechanical pulp cores. Taber stiffness testing measures the bending moment required to deflect a specimen by fifteen degrees.
Internal bond strength determines whether plies act as a unified beam or slide independently.
Creasing Strain
Internal shear stress develops during rotary scoring and flatbed die-cutting operations. Controlling layer deflection during scoring prevents liner ruptures on the outer face while creating clean, repeatable fold lines. Deep score impressions force outer plies into tension and inner plies into compression.
Inadequate delamination within core layers prevents stress relief, causing cracking along creased edges.
Board Failure
High flexural resistance ensures folding cartons maintain square shapes during high-speed cartoning line operations. Substrates exhibiting improper layer deflection collapse under side-seam compression or bulge when filled with dense granular products. Ply separation during bending reduces overall package stackability in transit.
Converting plants adjust score width and depth according to board thickness to optimize crease bending ratios. Humidity variations alter inter-ply cohesion and change bending performance. Crease stiffness testing verifies score quality before high-speed carton erecting.