Coating Flaw
Small microscopic cavities that penetrate through a dried coating layer expose the underlying fiber substrate to air and moisture. These defects, designated as surface pinholes, occur during the application or drying of liquid coatings on paper and paperboard. They compromise the barrier performance and appearance of the material.
Formation Mechanism
Air bubbles entrained in the wet coating mixture migrate toward the surface as the sheet dries. If the viscosity of the coating is too high, these bubbles cannot escape cleanly, or they pop too late, leaving a hollow crater that does not heal before the layer solidifies. Poor surface wetting of the paperboard can also cause the liquid to withdraw from certain points, creating identical microscopic voids.
Ensuring adequate deaeration of the coating color prevents bubble formation.
Quality Consequence
Defects in the coating barrier lead to severe printing and functional issues in the final package. When printing with ink, these voids cause localized speckling where the ink cannot transfer to the missing surface, resulting in poor color density and image quality. In barrier-coated packaging, these microscopic openings allow grease, water, or gases to penetrate the board, which reduces the shelf life of the packaged food products.
Using proper defoaming agents and adjusting the drying rate helps maintain a continuous, defect-free barrier layer.