Test Protocol
Standardized testing procedures of this class define the method for determining the ink rub resistance of printed paperboard using a reciprocating rub tester. The TAPPI T 830 provides a consistent protocol for evaluating the durability of printed packaging materials under controlled rubbing conditions. This standard is widely used by manufacturers and buyers to verify the print quality of shipping containers.
Machine Operation
Execution of the test requires cutting a printed specimen and a standard receptor block to the specified dimensions and mounting them in the tester. The tester moves a weighted receptor block back and forth across the printed specimen for a set number of cycles. The amount of ink transferred to the receptor is then evaluated using a densitometer or by comparison to reference standards.
This procedure is repeated for dry and wet rub tests to simulate different shipping environments.
Protocol Limit
Achieving consistent results demands that the test is performed in a temperature and humidity controlled room to maintain stable board conditions. This standard does not apply to unprinted boards or to coatings that do not contain pigments. The results can be affected by the ink used and the surface roughness of the paperboard.
Regular maintenance and calibration of the tester are required to ensure compliance with the standard.