Internal Bond Test
Dynamic pendulum impact measurement quantifies the internal z-directional delamination resistance of paper, paperboard, and multi-ply structures. Published by the Technical Association of the Pulp and Paper Industry, TAPPI T569 standardizes the determination of Scott bond energy by measuring the work required to cleave a paper sample glued between an aluminium angle and a rigid base plate. A weighted pendulum swings through a calibrated arc, striking the upright flange of the angle piece and ripping the paper specimen apart along its weakest internal plane.
The loss in pendulum kinetic energy directly reflects the internal bond strength of the fibrous matrix, recorded in Joules per square meter. The standard applies to paperboards subjected to rapid out-of-plane forces, but ceases to yield reproducible data on high-stretch substrates or sheets that fail to bond uniformly to double-sided tape.
Specimen Preparation Procedure
Testing requires five calibrated metal specimen bases and matching aluminium ninety-degree impact angles mounted inside a standardized mechanical preparation station. TAPPI T569 specifies applying heavy-duty, double-coated pressure-sensitive adhesive tape between the clean metal base, the test sheet, and the impact angle. A pneumatic or mechanical press applies uniform compressive load across the sample assembly for a defined dwell time to guarantee consistent adhesive wetting without crushing the paper’s internal pore structure.
The assembly is latched into the test instrument, where an inverted pendulum releases from an angle of zero degrees, falling under gravity to impact the horizontal flange. The pointer or electronic encoder registers the maximum follow-through height, translating mechanical work into internal bond energy.
Converting Suitability
High-tack offset lithography subjects paperboard to intense perpendicular surface peel forces as the ink-laden blanket releases the sheet. Compliance with TAPPI T569 verifies that paperboard will not experience ply separation or fiber blistering under high printing tack and rapid press speeds. Multi-ply folding boxboard requires minimum internal bond values around one hundred and fifty Joules per square meter to resist edge splits during high-speed scoring and folding.
Packaging lines producing pharmaceutical cartons rely on these impact values to confirm that creased carton flaps fold square and maintain structural integrity during automatic cartoning operations.