Film Cohesion
Pinholes, fissures and uncoated micro-voids across a treated paper or board surface determine the boundary where a protective layer ceases to act as an uninterrupted physical shield. Measuring barrier coating continuity establishes whether an applied aqueous dispersion, extruded biopolymer or synthetic resin forms an unbroken film across raw cellulose fibres. Such continuity governs resistance against mineral oils, grease, liquid water and water vapour migration.
Surface roughness, coating rheology and drying dynamics govern this morphology. When base sheet fibres poke through the dried film, localized failure points emerge.
Verification Method
Standardized dye penetration tests, electrical conductivity sensing and scanning electron microscopy detect breaks across treated surfaces. In greaseproof evaluation, solvent-based turpentine or oil solutions colored with spirit dyes identify discrete breaches through visible wicking patterns. Water-based conductive solutions paired with low-voltage electrodes measure current leakage through unsealed paths to quantify void frequency per square metre.
Base sheet formation uniformity strongly alters local coat weight distribution, meaning areas of low grammage often present incomplete coverage. High calendering smooths surface hills to decrease peak-to-valley depths before chemical application.
Forming Tolerance
Scoring, creasing and edge folding impose tensile stresses that rupture brittle polymer layers. Barrier coating continuity drops sharply along the outer hinge of folded carton blanks when tensile elongation limits fall below local substrate strain. Plasticizing additives and flexible co-binders preserve continuity along critical 180-degree carton creases.
Unconverted flat sheet values do not guarantee packaged box integrity once converting lines introduce shear forces. Defective seals permit rapid product oxidation or moisture loss during pallet storage.