Dimensional Change
Thickness increases in paper and board occur when the internal fibre network absorbs moisture from the surrounding environment. The out of plane swelling describes the expansion of a sheet in the z-direction, perpendicular to the surface of the paper. This phenomenon is more pronounced than expansion in the machine or cross directions because the fibres are oriented primarily in the plane of the sheet.
Stresses created during the drying process at the paper mill are released when the substrate is re-moistened, leading to a permanent change in caliper.
Printing Impact
Register errors and feeding issues often arise when a substrate undergoes rapid moisture absorption during a multi-stage process. In inkjet printing, the application of water-based inks can trigger an immediate out of plane swelling that causes the paper to wave or cockle. This can lead to the sheet striking the print head or causing jams in the transport mechanism.
Precise humidity control in the press room is the primary method used to mitigate these structural changes.
Structural Consequence
Laminated structures and coated boards are particularly sensitive to internal expansion. When the core of a board expands, the out of plane swelling can cause delamination if the internal bond strength is insufficient. Coated surfaces may crack if the base sheet expands at a different rate than the rigid coating layer.
In liquid packaging board, this expansion must be managed to ensure the integrity of the barrier layers. Packaging designers must account for these changes when specifying tolerances for tight-fitting components. Even a small increase in caliper can result in a friction fit that prevents automated machinery from assembling a carton correctly.