Internal Strength
Standardized mechanical testing measures the internal bond strength of paper and board perpendicular to the sheet surface. Laboratory testing according to z-direction tensile ISO 15754 determines the force required to pull paperboard plies apart under pure tensile load applied normal to the sheet plane. Double-sided adhesive tape attaches double metal platens to test specimen surfaces before a tensile testing machine applies perpendicular force until structural failure occurs.
The resulting measurement quantifies internal z-direction cohesion necessary for blister packaging and creasing resistance.
Stress Distribution
Uniform adhesive bonding between metal platens and paperboard test pieces prevents stress concentrations that cause premature sample failure. Tensile testing crossheads pull the upper platen upward at constant elongation rates, transmitting uniform tensile stress across the thickness of the paper sample. Tensile forces strain fiber-to-fiber hydrogen bonds and inter-ply interfaces until the weakest structural zone within the paperboard matrix ruptures.
Maximum recorded peak force divided by test piece cross-sectional area yields internal bond strength values expressed in kilopascals. Fiber furnish refining level, wet press consolidation, ply bonding starches and sheet density dictate internal tensile resistance values recorded during standardized testing.
Fiber Boundary
Tape adhesion failure during tensile testing invalidates test results when platen adhesive bond strength falls below sheet internal strength. Test specimens with high surface roughness or loose surface dust prevent uniform tape adhesion, leading to false low tensile readings. Compliance with z-direction tensile ISO 15754 requires rigid sample mounting and strict climate conditioning at standard testing atmospheres.