Intermolecular Disruption
Cohesive separation occurs within the fibrous network when mechanical stress, moisture penetration or thermal agitation breaks the electrostatic bonds linking hydroxyl groups on adjacent cellulose microfibrils. In dry tensile and tear testing of paper substrates, hydrogen bond rupture marks the primary mechanism of internal network failure before individual fibre fracture occurs. This bond dissociation governs the yielding behavior of paperboard under load, determining the initial slope change on stress-strain curves.
The boundary of this reaction ends where irreversible mechanical separation triggers macroscopic sheet failure or complete network disintegration.
Dissociation Mechanics
Tensile loading straightens naturally curled fibres inside the sheet, concentrating shear stresses across the bonded contact areas where individual fibre walls overlap. Cellulose surfaces adhere via hydroxyl interactions across Campbell-force-consolidated contact zones during wet pressing and drying. As external loading exceeds the bond dissociation energy of roughly twenty kilojoules per mole, adjacent cellulose chains slide apart microscopically.
If ambient water enters the matrix, water molecules compete for hydroxyl bonding sites, forming secondary hydrogen bonds that drastically reduce dry network strength.
Mechanical Cohesion
Wet-strength additives like polyamide-epichlorohydrin resins counteract this rupture process by building water-resistant covalent crosslinks around existing fibre junctions. Under unconstrained loading, hydrogen bond rupture generates micro-cracks that propagate rapidly across the sheet matrix, lowering final bursting strength and internal Scott bond resistance. High-speed web tension adjustments on converting equipment must maintain stresses well below the critical threshold for widespread bond dissociation to prevent unexpected web breaks.
Controlling pressing uniformity during papermaking maximizes the initial bonded area, delaying rupture under conversion strains.